Aluminium alloy 3004 is a non-heat-treatable alloy known for its excellent formability, good corrosion resistance, and moderate strength. While it may not be the most common choice for chequered sheets or plates in structural applications due to its softer nature, it is often used in applications where these properties are beneficial.
Details and Characteristics: |
---|
Formability: 3004 aluminium alloy is highly formable, making it suitable for applications where shaping, bending, or deep drawing is required. Corrosion Resistance: 3004 exhibits good corrosion resistance, making it suitable for applications exposed to mild corrosive conditions. Applications: Beverage cans and can ends Roofing and siding materials Cooking utensils Heat exchangers Chemical and food processing equipment |
Alloy : 3004 Aluminium Alloy
Temper:
O / F / H12 H14 H16 H18 H19 H22 H24 H26 H32 H34 H36 H38 H111 H112 H321 / T3 T4 T5 T6 T7 T351 T451 T651 T851
Thickness: 0.2mm - 10mm
Width: 500mm-2000mm
Standard: GB/T 3880-2012 ASTMB209 EN485
Pattern: Big Five Bars / Small Five Bars / Two Bars/ Small Three Bars / Diamond
Surface Treatment: Mill Finish / Brush Polish / Bright Finish
MOQ: The inventory has no MOQ 2mt-3mt
Packing: Standard Export Packing
Port of Dispatch: It depends on the supplier's location and shipping arrangements
Delivery Time: The inventory is 5-7 days . 25-30 days for customized products
Payment: TT / LC / TT+LC
Chemical Composition |
|
Aluminium (Al): | 95.8% |
---|---|
Copper (Cu): | 0.3% |
Iron (Fe): | 0.7% |
Manganese (Mn): | 1.0-1.5% |
Magnesium (Mg): | 0.8-1.3% |
Zinc (Zn): | 0.25% |